Standard

The Origin of Synergetic Effect in Mixed Mn-Co Oxide with Spinel Structure for Catalytic Oxidation of CO. / Bulavchenko, Olga A.; Rogov, Vladimir A.; Gerasimov, Evgeny Yu и др.

в: Inorganics, Том 13, № 1, 8, 31.12.2024.

Результаты исследований: Научные публикации в периодических изданияхстатьяРецензирование

Harvard

APA

Vancouver

Bulavchenko OA, Rogov VA, Gerasimov EY, Aydakov EE, Kremneva AM. The Origin of Synergetic Effect in Mixed Mn-Co Oxide with Spinel Structure for Catalytic Oxidation of CO. Inorganics. 2024 дек. 31;13(1):8. doi: 10.3390/inorganics13010008

Author

BibTeX

@article{aa76af86ce1a499c944e18b7095a9df9,
title = "The Origin of Synergetic Effect in Mixed Mn-Co Oxide with Spinel Structure for Catalytic Oxidation of CO",
abstract = "In this work, the origin of the synergetic effect in mixed MnxCo3-xO4 oxides with the spinel structure in the CO oxidation reaction was tested. A series of MnxCo3-x oxide catalysts were synthesized by the coprecipitation method with further calcination at 600 °C and varying manganese content from x = 0 to x = 3. The catalysts were characterized using XRD, TEM, N2 adsorption, TPR, EXAFS, and XPS. The catalytic activity of MnxCo3-x oxide catalysts was tested in CO oxidation reactions. The addition of manganese to cobalt oxide results in the formation of mixed Mn-Co oxides based on a cubic or tetragonal spinel structure, a change in microstructural properties, such as surface area and crystal size, as well as local distortions and a decrease in the surface concentration of Co ions and Co in the octahedral sites in spinel structure; it also decreases catalyst reducibility. For all catalysts, the activity of CO oxidation decreases as follows: Mn0.1Co2.9 > Co3O4~Mn0.3Co2.7 > Mn0.5Co2.5 > MnOx > Mn0.7Co2.3 > Mn0.9Co2.1~Mn1.1Co1.9~Mn2.5Co0.5 > Mn2.9Co0.1 > Mn1.7Co1.3 > Mn2.1Co0.9 > Mn1.3Co1.7~Mn1.5Co1.5~Mn2.3Co0.7. The Mn0.1Co2.9 catalyst displays the best catalytic activity, which is attributed to its small crystal size and the maximum surface ratio between Co3+ and Co2+. A further increase in the manganese content (x > 0.3) provokes drastic changes in the catalytic properties due to a decrease in the cobalt content on the surface and in the volume of mixed oxide, changes in the oxidation states of cations, and structure transformation.",
keywords = "CO oxidation, MnxCo3-xO4 oxides, solid solutions, synergetic effect",
author = "Bulavchenko, {Olga A.} and Rogov, {Vladimir A.} and Gerasimov, {Evgeny Yu} and Aydakov, {Egor E.} and Kremneva, {Anna M.}",
note = "This work was supported by the Ministry of Science and Higher Education of the Russian Federation (Grant Agreement No. 075-15-2022-263).",
year = "2024",
month = dec,
day = "31",
doi = "10.3390/inorganics13010008",
language = "English",
volume = "13",
journal = "Inorganics",
issn = "2304-6740",
publisher = "Multidisciplinary Digital Publishing Institute (MDPI)",
number = "1",

}

RIS

TY - JOUR

T1 - The Origin of Synergetic Effect in Mixed Mn-Co Oxide with Spinel Structure for Catalytic Oxidation of CO

AU - Bulavchenko, Olga A.

AU - Rogov, Vladimir A.

AU - Gerasimov, Evgeny Yu

AU - Aydakov, Egor E.

AU - Kremneva, Anna M.

N1 - This work was supported by the Ministry of Science and Higher Education of the Russian Federation (Grant Agreement No. 075-15-2022-263).

PY - 2024/12/31

Y1 - 2024/12/31

N2 - In this work, the origin of the synergetic effect in mixed MnxCo3-xO4 oxides with the spinel structure in the CO oxidation reaction was tested. A series of MnxCo3-x oxide catalysts were synthesized by the coprecipitation method with further calcination at 600 °C and varying manganese content from x = 0 to x = 3. The catalysts were characterized using XRD, TEM, N2 adsorption, TPR, EXAFS, and XPS. The catalytic activity of MnxCo3-x oxide catalysts was tested in CO oxidation reactions. The addition of manganese to cobalt oxide results in the formation of mixed Mn-Co oxides based on a cubic or tetragonal spinel structure, a change in microstructural properties, such as surface area and crystal size, as well as local distortions and a decrease in the surface concentration of Co ions and Co in the octahedral sites in spinel structure; it also decreases catalyst reducibility. For all catalysts, the activity of CO oxidation decreases as follows: Mn0.1Co2.9 > Co3O4~Mn0.3Co2.7 > Mn0.5Co2.5 > MnOx > Mn0.7Co2.3 > Mn0.9Co2.1~Mn1.1Co1.9~Mn2.5Co0.5 > Mn2.9Co0.1 > Mn1.7Co1.3 > Mn2.1Co0.9 > Mn1.3Co1.7~Mn1.5Co1.5~Mn2.3Co0.7. The Mn0.1Co2.9 catalyst displays the best catalytic activity, which is attributed to its small crystal size and the maximum surface ratio between Co3+ and Co2+. A further increase in the manganese content (x > 0.3) provokes drastic changes in the catalytic properties due to a decrease in the cobalt content on the surface and in the volume of mixed oxide, changes in the oxidation states of cations, and structure transformation.

AB - In this work, the origin of the synergetic effect in mixed MnxCo3-xO4 oxides with the spinel structure in the CO oxidation reaction was tested. A series of MnxCo3-x oxide catalysts were synthesized by the coprecipitation method with further calcination at 600 °C and varying manganese content from x = 0 to x = 3. The catalysts were characterized using XRD, TEM, N2 adsorption, TPR, EXAFS, and XPS. The catalytic activity of MnxCo3-x oxide catalysts was tested in CO oxidation reactions. The addition of manganese to cobalt oxide results in the formation of mixed Mn-Co oxides based on a cubic or tetragonal spinel structure, a change in microstructural properties, such as surface area and crystal size, as well as local distortions and a decrease in the surface concentration of Co ions and Co in the octahedral sites in spinel structure; it also decreases catalyst reducibility. For all catalysts, the activity of CO oxidation decreases as follows: Mn0.1Co2.9 > Co3O4~Mn0.3Co2.7 > Mn0.5Co2.5 > MnOx > Mn0.7Co2.3 > Mn0.9Co2.1~Mn1.1Co1.9~Mn2.5Co0.5 > Mn2.9Co0.1 > Mn1.7Co1.3 > Mn2.1Co0.9 > Mn1.3Co1.7~Mn1.5Co1.5~Mn2.3Co0.7. The Mn0.1Co2.9 catalyst displays the best catalytic activity, which is attributed to its small crystal size and the maximum surface ratio between Co3+ and Co2+. A further increase in the manganese content (x > 0.3) provokes drastic changes in the catalytic properties due to a decrease in the cobalt content on the surface and in the volume of mixed oxide, changes in the oxidation states of cations, and structure transformation.

KW - CO oxidation

KW - MnxCo3-xO4 oxides

KW - solid solutions

KW - synergetic effect

UR - https://www.mendeley.com/catalogue/1c99b054-6a71-37fb-9692-26ada5660a0a/

UR - https://www.scopus.com/record/display.uri?eid=2-s2.0-85216210283&origin=inward&txGid=7855c4c82f221ef762a91a1697afe8a1

U2 - 10.3390/inorganics13010008

DO - 10.3390/inorganics13010008

M3 - Article

VL - 13

JO - Inorganics

JF - Inorganics

SN - 2304-6740

IS - 1

M1 - 8

ER -

ID: 63949995