Effect of the Calcination Temperature and Composition of the MnOx–ZrO2 System on Its Structure and Catalytic Properties in a Reaction of Carbon Monoxide Oxidation. / Afonasenko, T. N.; Bulavchenko, O. A.; Gulyaeva, T. I. и др.
в: Kinetics and Catalysis, Том 59, № 1, 01.01.2018, стр. 104-111.Результаты исследований: Научные публикации в периодических изданиях › статья › Рецензирование
}
TY - JOUR
T1 - Effect of the Calcination Temperature and Composition of the MnOx–ZrO2 System on Its Structure and Catalytic Properties in a Reaction of Carbon Monoxide Oxidation
AU - Afonasenko, T. N.
AU - Bulavchenko, O. A.
AU - Gulyaeva, T. I.
AU - Tsybulya, S. V.
AU - Tsyrul’nikov, P. G.
PY - 2018/1/1
Y1 - 2018/1/1
N2 - The effect of the calcination temperature and composition of the MnOx–ZrO2 system on its structural characteristics and catalytic properties in the reaction of CO oxidation was studied. According to X-ray diffraction analysis and H2 thermo-programmed reduction data, an increase in the calcination temperature of Mn0.12Zr0.88O2 from 450 to 900°C caused a structural transformation of the system accompanied by the disintegration of solid solution with the release of manganese ions from the structure of ZrO2 and the formation of, initially, highly dispersed MnOx particles and then a crystallized phase of Mn3O4. The dependence of the catalytic activity of MnOx–ZrO2 in the reaction of CO oxidation on the calcination temperature takes an extreme form. A maximum activity was observed after heat treatment at 650–700°C, i.e., at limiting temperatures for the occurrence of a solid solution of manganese ions in the cubic modification of ZrO2. If the manganese content was higher than that in the sample of Mn0.4Zr0.6O2, the phase composition of the system changed: the solid solution phase was supplemented with Mn2O3 and β-Mn3O4 phases. The samples of Mn0.4Zr0.6O2–Mn0.6Zr0.4O2 exhibited a maximum catalytic activity; this was likely due to the presence of the highly dispersed MnOx particles, which were not the solid solution constituents, on their surface in addition to an increase in the dispersity of the solid solution.
AB - The effect of the calcination temperature and composition of the MnOx–ZrO2 system on its structural characteristics and catalytic properties in the reaction of CO oxidation was studied. According to X-ray diffraction analysis and H2 thermo-programmed reduction data, an increase in the calcination temperature of Mn0.12Zr0.88O2 from 450 to 900°C caused a structural transformation of the system accompanied by the disintegration of solid solution with the release of manganese ions from the structure of ZrO2 and the formation of, initially, highly dispersed MnOx particles and then a crystallized phase of Mn3O4. The dependence of the catalytic activity of MnOx–ZrO2 in the reaction of CO oxidation on the calcination temperature takes an extreme form. A maximum activity was observed after heat treatment at 650–700°C, i.e., at limiting temperatures for the occurrence of a solid solution of manganese ions in the cubic modification of ZrO2. If the manganese content was higher than that in the sample of Mn0.4Zr0.6O2, the phase composition of the system changed: the solid solution phase was supplemented with Mn2O3 and β-Mn3O4 phases. The samples of Mn0.4Zr0.6O2–Mn0.6Zr0.4O2 exhibited a maximum catalytic activity; this was likely due to the presence of the highly dispersed MnOx particles, which were not the solid solution constituents, on their surface in addition to an increase in the dispersity of the solid solution.
KW - CO oxidation
KW - MnO–ZrO catalysts
KW - COMBUSTION
KW - MANGANESE OXIDES
KW - METHANE
KW - REDUCTION
KW - ZR OXIDES
KW - BEHAVIOR
KW - GAMMA-MNO2
KW - MnOx-ZrO2 catalysts
KW - LATTICE OXYGEN
UR - http://www.scopus.com/inward/record.url?scp=85043280833&partnerID=8YFLogxK
U2 - 10.1134/S0023158418010019
DO - 10.1134/S0023158418010019
M3 - Article
AN - SCOPUS:85043280833
VL - 59
SP - 104
EP - 111
JO - Kinetics and Catalysis
JF - Kinetics and Catalysis
SN - 0023-1584
IS - 1
ER -